ABS AH40 |
BV AH40 |
CCS AH40 |
DNV AH40 |
GL AH40 |
KR AH40 |
LR AH40 |
NK AH40 |
RINA AH40 |
C max |
Mn |
Si |
P max |
S max |
Al max. |
Cb |
V |
Ti max. |
Cu max. |
Cr max. |
Ni max. |
Mo max. |
0.18 |
0.90-1.60 |
0.10-0.50 |
0.035 |
0.035 |
0.015 |
0.02-0.05 |
0.05-0.10 |
0.02 |
0.35 |
0.20 |
0.40 |
0.08 |
Yield Strength (MPa) min. |
Tensile Strength (MPa) |
Elongation in 8 in. min. % |
Elongation in 2 in. min. % |
390 |
510-650 |
19 |
22 |
1.The general hull structural steel grades A, B, D, and E are distinguished according to the impact temperature of the steel. The impact values of all grades of steel are the same, not according to the strength grade.
Grade A steel is the impact force subjected to normal temperature (20 ° C).
Grade B steel is the impact force at 0 °C.
Grade D steel is the impact force at -20 °C.
Grade E steel is the impact force at -40 °C.
High-strength hull structural steel can be further divided into AH32, DH32, EH32, AH36, DH36, EH36
2, high-intensity hull structure steel preheating requirements: all AH, DH, EH plate thickness greater than 30mm angle, butt joints, preheating to 120 ~ 150 °C before welding.
3, the thickness of the plate ≤ 30mm, the ambient temperature is below 5°C, preheated to 75 °C; ambient temperature below 0 °C, preheated to 75 ~ 100 °C.
4, TMCP steel (made in Japan), and it is cannot preheat before welding.
We have our own processing factory and the pre- treatment factory, pre-treatment for shipbuilding steel, Surface pretreatment line technical parameters on RINA AH40 steel plates and profile steel. And we can also make the customers enjoy our other pre-treatment services, like cutting, welding, drilling holes by the lowest cost price. Besides, We are a professional RINA AH40 Shipbuilding Steel exporter and stockist in china. Any need please feel free to contact us.