The CCS Grade AH36 and CCS Grade DH36 shipbuilding steel plates have yield strength of 51,000 psi (355 MPa), and ultimate tensile strength of 71,000 - 90,000 psi (490-620 MPa). All the CCS Grade AH36 steel plates, CCS Grade DH36 shipbuilding Steel offered by Katalor Industry can be certificated by China Classification Society(CCS) as per customer’s request.
There are subtle difference bewteen CCS Grade AH36 and CCS Grade DH36.
CCS Grade AH36 Steel Vs CCS Grade DH36 Steel
CCS AH36 Steel Chemical Composition (%, by weight)
C max | Mn | Si | P max | S max | Al max. | Cb | V | Ti max. | Cu max. | Cr max. | Ni max. | Mo max. |
0.18 | 0.90-1.60 | 0.10-0.50 | 0.035 | 0.035 | 0.015 | 0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
C max | Mn | Si | P max | S max | Al max. | Cb | V | Ti max. | Cu max. | Cr max. | Ni max. | Mo max. |
0.18 | 0.90-1.60 | 0.10-0.50 | 0.035 | 0.035 | 0.015 | 0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |