The ABS AH36 and ABS DH36 grades have yield strength of 51,000 psi (355 MPa), and ultimate tensile strength of 71,000 - 90,000 psi (490-620 MPa). All the ABS AH36 steel plates, ABS DH36 shipbuilding steel offered by Katalor Industry can be certificated by American Bureau of Shipping(ABS) as per customer’s request.
There are subtle difference bewteen ABS AH36 and ABS DH36.
ABS AH36 Steel Chemical Composition (%, by weight)
C max | Mn | Si | P max | S max | Al max. | Cb | V | Ti max. | Cu max. | Cr max. | Ni max. | Mo max. |
0.18 | 0.90-1.60 | 0.10-0.50 | 0.035 | 0.035 | 0.015 | 0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |
C max | Mn | Si | P max | S max | Al max. | Cb | V | Ti max. | Cu max. | Cr max. | Ni max. | Mo max. |
0.18 | 0.90-1.60 | 0.10-0.50 | 0.035 | 0.035 | 0.015 | 0.02-0.05 | 0.05-0.10 | 0.02 | 0.35 | 0.2 | 0.4 | 0.08 |